Snowdon Visitors Center
At 1,085 metres, this unique visitor centre is one of the highest building in the UK, responding to one of the most extreme climatic locations: the mountain endures facing winds of 120mph, temperatures that can go below -200C and 5 m of rain every year. The list of special design considerations for this unique project is endless - life cycle costs, building life, sustainable development and complex design considerations.
Posted on Saturday, March 5, 2011
Case Study File -
The Bridge of Sustainability
For years, children in a Chinese community divided by the River Po – a tributary of the Yellow River – had to cross the river on a precarious single-log bridge: built on pillars of straw, rock and earth. Among the many accidents, a mother and child were swept to their deaths on the journey to the school on the other side of the waterway from their homes.
Posted on Saturday, March 5, 2011